Polyurea Elastomeric Coatings

Polyurea Elastomeric Coatings

Elastict polyurea microsphere coating
Chat Now

Product Details

Model:PA6376


Description 


Composition

A four-part coating cured by aspartic   acid ester resin and isocyanateadded organic   particle aggregate and thinner.

Curing method

Normal tempetature curing,0-35℃.

Application

Elastic floor coatings cover glossy   finish.

Features

 

High solid content, low toxicity and   environmental protection, excellent weather resistance, good rebound,   excellent scratch resistance and abrasion resistance.

Package

A agent 3.29kg, B agent 0.65kg, C agent 0.82kg, D agent 0.23kg.         (ratio 100:20:25:7)

Range of use

Mainly used in schools, hospitals,   playgrounds and other flexible floor coverings to improve the wear   resistance, scratch resistance, and weatherability and yellowing resistance.



Material base data(25℃,60%RH)




A Agent

B  Agent

 

Appearance

Colorless   liquid

Light   yellow liquid

Smell

Non

Slight

Viscosity25

1400MPaS

12MPaS

Proportion25

1.1


Solid content

95%   





Mixed material Data(25℃,60%RH)    


Viscosity of mixed : 800MPaS

Mixing proportion (without aggregate):1.05

Mixed solids(with aggregate):83%

Potlife : 20min   

Dry time:2hr                   

Walking Opening time: 8hr

Weight opening time: 48days

Operation time and temperature relation

Material physical properties after curing



Operation time and temperature relation



10

25℃,50%RH

30℃,75%RH

Usable time

30min

20min

15min

Finger touch

4hr

2.5hr

2hr

Tack Free

16hr

8hr

6hr



Material physical properties after curing



Paint film apperance

Semi-matt light skid-resistant surface

7th   hardness

HB

Wear(CS17 wheel 750g,500 turn)

20mg

Anti-impact performance          1000g1m

Pass



Attention:  


Construction prohibited when humidity is greater than 85%RH;

The curing agent component meets the water vapor extremely easily to deteriorate, saves must seal dry.



User's guidance: 


After mixing, the material must be poured all over the floor and then scraped, so as to avoid the bottom of the aggregate and the poor surface effect;

Adopt the construction method of batch scraping firstly and then roller coating, and evenly collect the short wool or sponge roller;

Dosage strictly controlled in 0.08~0.1kg/m2, avoidaccumulation, otherwise foaming serious;

This material has very high requirements for construction. It must be trained by our company before use.



Storage: Ideal storage conditions is 5-35 ℃ in cool and dry place, avoid sun exposure.